Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 16.482 MPa-m½ | 15.000 ksi-in½ | T-L |
Kaiser 7068 T6, T6511 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |