Fracture Toughness 1.83 MPa-m½
1.67 ksi-in½
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix
HexPly® M42 is a high performance, self extinguishing, self adhesive, tough epoxy matrix for use in primary aerospace sandwich structures. It exhibits very high impact resistance and damage toleran..