Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 2.00 MPa-m½ | 1.82 ksi-in½ | Notched Beam |
CoorsTek Mullite, S2 Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Fracture Toughness | 2.00 MPa-m½ | 1.82 ksi-in½ | |
CoorsTek Porcelain Information provided by CoorsTek. |