Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 1.62 MPa-m½ | 1.47 ksi-in½ | |
Hexcel® HexPly® 8552 Epoxy Matrix HexPly® 8552 is an amine cured, toughened epoxy resin system supplied with unidirectional or woven carbon or glass fibers. HexPly® 8552 is recommended for structural applications requiring high st.. |