Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 1.53 MPa-m½ | 1.39 ksi-in½ | |
Corning Macor® Machinable Glass Ceramic The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,.. |
|||
Fracture Toughness | 1.53 MPa-m½ | 1.39 ksi-in½ | |
Accuratus MACOR Machinable Glass Ceramic Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac.. |
|||
Fracture Toughness | 1.53 MPa-m½ | 1.39 ksi-in½ | |
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |