Polymer Property : Fracture Toughness = 1.11 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 1.22 MPa-m½
1.11 ksi-in½
Hexcel® HexPly® F593 Epoxy Resin
HexPly® F593 is a modified 350°F (177°C) curing epoxy system with very low flow for carbon fabric and tape applications that provides excellent laminate and honeycomb sandwich properties. As a lo..