Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 0.433 - 3.69 MPa-m½ | 0.394 - 3.36 ksi-in½ | Average value: 1.33 MPa-m½ Grade Count:18 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Fracture Toughness | 0.433 MPa-m½ | 0.394 ksi-in½ | |
Hexcel® F161 Epoxy Resin F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is.. |