Polymer Property : Tensile Modulus = 998 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.88 GPa
998 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC
LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber.
Tensile Modulus 6.88 GPa

@Temperature -40.0 °C
998 ksi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes..