Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.86 GPa | 996 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GR-4030 ABS, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 6.86 GPa | 996 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GR-4030 ABS, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 6.87 GPa | 996 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PH0390A PA 6 LNP THERMOCOMP* PH0390A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |