Mechanical Properties Metric English Comments
Tensile Modulus 6.62 GPa
960 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® TR2-30GF/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
Tensile Modulus 6.62 GPa
960 ksi
ISO 527 Type 1A
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 50
Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin..
Tensile Modulus 6.62 GPa
960 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC
LNP THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Flame Retardant.
Tensile Modulus 6.62 GPa
960 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC (Asia Pacific)
LNP* THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.
Tensile Modulus 6.62 GPa
960 ksi
ASTM D638
Asahi Kasei Thermylene® P6-30FG-0570 30% Glass Fiber Reinforced, Flame Retardant