Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 64.8 GPa @Temperature 23.9 °C |
9400 ksi @Temperature 75.0 °F |
0° Direction, Dry, 365° Oven Cured; ASTM D3039 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 12K PW HTS Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |