Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.648 GPa | 94.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.648 GPa | 94.0 ksi | Sintered Molding; ASTM D638 |
3M Dyneon™ TFM™ 1630 PTFE
(discontinued **) Semi-free-flowing resin for convenient handlingHigh bulk density leading to more economical processingVery dense polymer structure; low permeabilityGood electrical and mechanical propertiesSmoother .. |
|||
Tensile Modulus | 0.648 GPa | 94.0 ksi | ASTM D638 |
3M Dyneon™ TFM™ X 1630 PTFE
(discontinued **) Semi-free-flowing resin for convenient handlingHigh bulk density leading to more economical processingVery dense polymer structure; low permeabilityGood electrical and mechanical propertiesSmoother .. |