Polymer Property : Tensile Modulus = 9300 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 64.1 GPa
9300 ksi
Greene Tweed Xycomp® 1030-02 Carbon/Nylon 12 Composite
Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st..