Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.325 GPa @Temperature -20.0 °C |
917.4 ksi @Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6
(Unverified Data**) 15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |