Tensile Modulus 0.630 GPa
91.4 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HP2EU PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol..
Tensile Modulus 0.630 GPa
91.4 ksi
MD; ASTM D882
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..