Polymer Property : Tensile Modulus = 90.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 90.0 - 120 GPa
13100 - 17400 ksi
Goodfellow Phosphor Bronze
Good Machinability. Uses include springs, clips, gauzes and architectural applicationsInformation provided by Goodfellow.