Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.93 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC LNP* LUBRICOMP* DFL369XF is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Tensile Modulus | 9.93 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific) LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant. |