Polymer Property : Tensile Modulus = 9.87 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 9.87 GPa
1430 ksi
ASTM D638
Plenco 4100 Phenolic, Granular, Compression Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and ..
Tensile Modulus 9.87 GPa
1430 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP KFL25 Acetal Copolymer
LNP LUBRICOMP* KFL25 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant.
Tensile Modulus 9.87 GPa
1430 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Asia Pacific)
LNP* Thermocomp* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber.
Tensile Modulus 9.87 GPa
1430 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp ZF-1006 BK8-950 PPE+PS
LNP* Thermocomp* ZF-1006 BK8-950 is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 9.87 GPa
1430 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP ZF-1006 BK8-950 PPE+PS (Asia Pacific)
LNP* Thermocomp* ZF-1006 BK8-950 is a compound based on PPE+PS Blend resin containing Glass Fiber.