Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.56 GPa | 1390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16 PA 6 LNP* LUBRICOMP* RFN16 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 9.56 GPa | 1390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16 PA 6 (Asia Pacific) LNP* Lubricomp* RFN16 is a compound based on Nylon 6 resin containing Glass Fiber, MOS2. Added features of this material include: Internally Lubricated. |