Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.41 GPa | 1360 ksi | same value from ASTM and ISO test. |
BASF Capron® HPN 9333G Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9333G is a 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface a.. |
|||
Tensile Modulus | 9.41 GPa | 1360 ksi | same value from ASTM and ISO test. |
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with.. |