Mechanical Properties Metric English Comments
Tensile Modulus 6.135 GPa
889.8 ksi
ISO 527-1/-2
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m..