Mechanical Properties Metric English Comments
Tensile Modulus 87.0 GPa
12600 ksi
Results normalized to 60% fibre volume for Carbon, 50% fibre volume for Kevlar; pr EN 2561 Type B
Hexcel® HexPly® 920CX-EP2015-47.5% 125°C Curing Epoxy Matrix
Intermediate modulus, 6K carbon, 2x2 twill, 193 g/m2Information provided by HexCel
Tensile Modulus 87.0 GPa
12600 ksi
Results normalized to 60% fibre volume for Carbon, 50% fibre volume for Kevlar; pr EN 2561 Type B
Hexcel® HexPly® 920CX-940-42% 125°C Curing Epoxy Matrix
Intermediate modulus, 6K carbon, 5H satin, 285 g/m2Information provided by HexCel