Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.799 GPa | 841.1 ksi | ASTM D638 |
Aclo Accutech ABS ABS831G40L Glass Reinforced |
|||
Tensile Modulus | 5.799 GPa | 841.1 ksi | ASTM D638 |
Aclo Accutech Polycarbonate POL051G40L Glass Reinforced |