Mechanical Properties Metric English Comments
Tensile Modulus 5.75 GPa
834 ksi
Plastcom SLOVAMID 6 T 30 TS PA6, 30% mineral filling
FeaturesDecreased shrinkage against the BT types, increased heat application. Increased modulus in tension - strength of the material. PA matrix reduction. PA for injection moulding with the content..