Mechanical Properties Metric English Comments
Tensile Modulus 5.74 GPa
833 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DX06411 PC
LNP* THERMOCOMP* DX06411 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.
Tensile Modulus 5.74 GPa
833 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DX06411 PC (Asia Pacific)
LNP* Thermocomp* DX06411 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.