Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.54 GPa | 1240 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP EX07305 PEI (Asia Pacific) Polyetherimide reinforced with Glass fiber and PTFE for use in Burn-in Test Sockets (BiTS) Application |
|||
Tensile Modulus | 8.54 GPa | 1240 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS (Asia Pacific) LNP* Thermocomp* CX05470 is a compound based on Polystyrene resin containing Glass Fiber. |
|||
Tensile Modulus | 8.54 GPa | 1240 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KFZ24XXP Acetal Copoly LNP* THERMOCOMP* KFZ24XXP is a compound based on Acetal Copolymer resin containing 20% Glass Fiber, 10% Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled, Inter.. |
|||
Tensile Modulus | 8.54 GPa | 1240 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing. |