Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.87 GPa | 706 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF PX06416 PA 6 LNP* Thermotuf* PX06416 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 4.87 GPa | 706 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF PX06416 PA 6 (Asia Pacific) LNP* Thermotuf* PX06416 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |