Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.99 GPa | 1160 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RX05495 PA 66 LNP LUBRICOMP* RX05495 is a compound based on Nylon 66 resin containing Glass Bead, Graphite, Glass Fiber. Added features of this material include: Easy Molding. |