Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0540 GPa | 7.83 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® G4078LS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Light ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.0540 GPa | 7.83 ksi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Tensile Modulus | >= 0.0540 GPa | >= 7.83 ksi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to .. |