Polymer Property : Tensile Modulus = 7.44 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 7.44 GPa
1080 ksi
50 mm/min; ASTM D638
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded
PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo..