Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.25 GPa | 1050 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP 2037/30 H2.0 LT 904040 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, black colored for laser transmission-welding (laser-transparent), good heat-ageing resistance |
|||
Tensile Modulus | 7.25 GPa | 1050 ksi | Film T.D.; ASTM D882 |
Eastman Eastman Embrace Copolyester for Shrink Film Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood .. |
|||
Tensile Modulus | 7.25 GPa | 1050 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR20 NL PA 6.6 20% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |