Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.24 GPa | 1050 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-NY-030-SS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 7.24 GPa | 1050 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Tensile Modulus | 7.24 GPa | 1050 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant. |
|||
Tensile Modulus | 7.24 GPa | 1050 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WF0039U PBT LNP* THERMOCOMP* WF0039U is a compound based on PBT resin containing 15% Glass Fiber. Added features of this grade include: Flame Retardant and UV Stabilized. |