Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 7.23 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 7.23 GPa
1050 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer
LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f..
Tensile Modulus 7.23 GPa
1050 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f..
Tensile Modulus 7.23 GPa
1050 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Asia Pacific)
LNP* Stat-kon* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.