Mechanical Properties Metric English Comments
Tensile Modulus 7.22 GPa
1050 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC (Asia Pacific)
LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.
Tensile Modulus 7.22 GPa
1050 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC
LNP LUBRICOMP* DFL349EF is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
Tensile Modulus 7.22 GPa
1050 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC
LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.