Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.470 GPa | 68.2 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 0.470 GPa | 68.2 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |