Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 67.0 GPa | 9720 ksi | EN2597B |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/40%/285T2/AS4C-6K Fiber: AS4C, Weave: 2x2T, 295 g/m2Information provided by HexCel |
|||
Tensile Modulus | 67.0 GPa | 9720 ksi | Material as cured; RT |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |
|||
Tensile Modulus | 67.0 GPa @Temperature 23.0 °C |
9720 ksi @Temperature 73.4 °F |
prEN2561 Type B |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/G1094/1000 Fiber: T800H 6K, 5H Satin weave, 290 g/m2Information provided by HexCel |