Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.528 GPa | 656.7 ksi | ISO 527 |
Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix AZDEL® C327-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |