Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.42 GPa | 641 ksi | ASTM D638 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 4.42 GPa | 641 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES LNP THERMOCOMP* JF002 is a compound based on Polyethersulfone resin containing 10% Glass Fiber. |