Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 64.0 GPa | 9280 ksi | |
Goodfellow Iron 40/Nickel 38/Boron 18 Alloy Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow. |
|||
Tensile Modulus | 64.0 GPa @Temperature 175 °C |
9280 ksi @Temperature 347 °F |
After ageing at 70°C / 95% RH |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |