Polymer Property : Tensile Modulus = 62400 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 430 GPa
62400 ksi
Young's; DINV ENV 843-2 / ASTM-F417
CeramTec Rocar® S Silicon Carbide, SSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..