Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.79 GPa | 985 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA6.12 LNP* THERMOCOMP* IF004 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 6.79 GPa | 985 ksi | ASTM D638 |
Plenco 51015 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by.. |