Polymer Property : Tensile Modulus = 6.53 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.53 GPa
947 ksi
ASTM D638
Plenco 51015 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by..