Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.47 GPa | 938 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF VF004S PA 66 LNP THERMOTUF* VF004S is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |