Polymer Property : Tensile Modulus = 6.27 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.27 GPa
910 ksi
ASTM D638
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet)
Tensile Modulus 6.27 GPa
909 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC
LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated.
Tensile Modulus 6.27 GPa
910 ksi
ASTM D638
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2..
Tensile Modulus 6.27 GPa

@Temperature 150 °C
909 ksi

@Temperature 302 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Tensile Modulus 6.27 GPa
909 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOTUF VFK33S PA 66
LNP THERMOTUF* VFK33S is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.
Tensile Modulus 6.27 GPa
910 ksi
ASTM D638
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire..
Tensile Modulus 6.27 GPa
909 ksi
50mm/min; ISO 527-2/1A
Celanese THERMX LED 0201 PCT, 40% Specialty
Thermx LED 0201 is a super white reinforced PCT resin highly suitable for LED applications. The material exhibits high heat resistance, high reflectance stability, high thermal stability, low moist..
Tensile Modulus 6.27 GPa

@Temperature 150 °C
909 ksi

@Temperature 302 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
Tensile Modulus 6.27 GPa
909 ksi
1mm/min; ISO 527-2/1A
Celanese Thermx® LED 0201 PCT, 40% Specialty  (Unverified Data**)
Thermx LED 0201 is a super white reinforced PCT resin highly suitable for LED applications. The material exhibits high heat resistance, high reflectance stability, high thermal stability, low moist..