Polymer Property : Tensile Modulus = 6.17 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.17 GPa
895 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS
LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare.
Tensile Modulus 6.17 GPa
895 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP AF004 ABS
LNP* THERMOCOMP* AF004 is a compound based on ABS resin containing 20% Glass Fiber.
Tensile Modulus 6.17 GPa

@Temperature 45.0 °C
895 ksi

@Temperature 113 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..