Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.04 GPa | 586 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 4.04 GPa | 586 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 4.04 GPa | 586 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |