Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.92 GPa | 569 ksi | |
TriStar Ultracomp UC-300 Composite Bearing Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family.. |