Polymer Property : Tensile Modulus = 567 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.91 GPa
567 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66
LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized.
Tensile Modulus 3.91 GPa
567 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 (Asia Pacific)
LNP* Lubricomp* RN001S is a compound based on Nylon 66 resin containing MOS2. Added features of this material include: Internally Lubricated, Heat Stabilized.
Tensile Modulus 3.91 GPa
567 ksi
ASTM D 638
Saint-Gobain Meldin® 3140 Thermoplastic Bearing Material
Meldin 3140 is an ideal thrust washer material and is well suited for thrust washer applications. Its high strength and stiffness, combined with its excellent heat dissipation properties, make it a..