Mechanical Properties Metric English Comments
Tensile Modulus 3.89 GPa
564 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Cycolac® INP564 ABS
SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Tensile Modulus 3.89 GPa
564 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycolac® INP564 ABS+SAN
SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Tensile Modulus 3.89 GPa
564 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp DF002L PC
LNP THERMOCOMP* DF002L is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC-IP for the America..
Tensile Modulus 3.89 GPa
564 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific)
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.
Tensile Modulus 3.89 GPa
564 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Xenoy® X6320 PBT+PC
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP..