Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 558 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.85 GPa
558 ksi
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling
FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode..
Tensile Modulus 3.85 GPa
558 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® FXE4271L PC (Asia Pacific)
Lexan* FXE4271L is a 10% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac..
Tensile Modulus 3.85 GPa
558 ksi
ISO 527-2/1A/1
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
Tensile Modulus 3.85 GPa
558 ksi
ISO 527-2/1A/1
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Tensile Modulus 3.85 GPa
558 ksi
1 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
Tensile Modulus 3.85 GPa
558 ksi
1 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
Tensile Modulus 3.85 GPa
558 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® X4850 PBT+PC
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Tensile Modulus 3.85 GPa
558 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Tensile Modulus 3.85 GPa
558 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Copyright © lookpolymers.com All Rights Reserved